Separation efficiency of different methods in treatment of a low-grade iron ore
Authors:
Özgür ÖZCAN
ABSTRACT
In the present study, characterization and beneficiation tests were performed on an iron ore sample for the evaluation of separation efficiency (SE) of different methods. Results showed that the decrease in feed size fraction increases the SE irrespective of to beneficiation method. It was determined from the liberation analyses that the increase in SE values at finer size fractions is related with higher liberation. Calculated SE values revealed that operational parameters significantly affect the SE of all methods and the net forces acting on particles play an important role on SE of different size fractions. Mean SE of different size fractions showed that the separation efficiencies of gravity concentration and magnetic separation takes similar values above 1 mm, however, SE of magnetic separation is significantly higher than gravity concentration below 1 mm for the studied sample. For low grade ores, it is very crucial to develop a flow sheet to achieve the optimum grade and recovery while decreasing the cost likely by using optimum method. Therefore, SE calculations used in this research can be used as a basic method to compare the efficiency of different beneficiation methods. SE method has advantages as they provide fast evaluation of efficiency by using experimental results.
Keywords:
Separation Efficiency Grade, Recovery, Magnetic Separation, Gravity Concentration.
In the present study a detailed characterization followed by beneficiation of low grade iron ore was studied. The Run of Mine (R.O.M) sample assayed 21.91 % Fe, which is very low grade in nature. The impurities are SiO2 26.25%, MgO 20.48%, CaO 5.85%, Al2O3 1.86% and loss on ignition (LOI) 12.71%. A Davis Tube test was performed for the assessment of the separability of magnetic ores by low intensity magnetic separators. The heavy liquid test was carried out to evaluate the possible response of the sample by the gravity concentration technique. The samples were subjected to jigging, dry low intensity magnetic separation (DLIMS) and shaking table tests. Thus a sufficient concentrate could not be obtained in +1 mm by using jigging and DLIMS. The obtained results show that the a high grade iron concentrate (>65% Fe) with lower recoveries was obtained from shaking table tests by using -1 mm fraction. According to the results a flowsheet was developed. From the developed flowsheet, it is possible to obtain pellet grade concentrate with 65.41% Fe, 2.54% SiO2, 2.79% MgO, 0.70% CaO and 0.32% Al2O3. with 21.42% weight recovery. The overall gangue rejection recovery of the circuit is over 95%.
https://doi.org/10.19111/bulletinofmre.834182
Keywords:
Low grade iron ore, Gravity concentration, Magnetic separation, Flowsheet development